8
Surface Mount Multilayer Ceramic Capacitors CC SERIES X7R, 16V to 100V
8
TEST AND REQUIREMENT
Table 9
IEC384-10 TEST ITEMS
4.9
Bending
4.10
Resistance to soldering heat
4.11
Solderability
4.12
Rapid change of temperature
4.14
Damp heat
4.15
Endurance
CONDITIONS
REQUIREMENTS
Bending rate 1mm/s, jig. radius 340mm ∆C/C≤10%
260±5°C for 10±0.5s in static solder
bath
–5%≤∆C/C≤10%
∆
235±5°C for 2±0.5s in a static solder
bath
75% minimum coverage of metallic area
Preconditioning
–55°C to +125°C, 5cycles
∆C/C within 15%
Preconditioning
At 40°C, 90 to 95% RH and Ur applied
(max. 500V) for 500 hours
∆C/C within 15%
Tan δ≤7%
IR≥500MΩ or RxC≥25s whichever is less
Preconditioning
2xUr applied for 1,000 hours, at upper
category temperature
∆C/C within 20%
Tan δ≤7%
IR≥1,000MΩ or RxC≥50s whichever is less